Epoxyden Primer Zinc Enrich Cold Galvanization
Epoxyden primer Zinc enrich anticorrosive recoatable
A two component anticorrosive recoat able epoxy primer enriched with zinc, suitable for painting ferrous metals in corrosive high level aggressive environment C5–I and complies with the standard ISO 12944-6 to chemicals (ISO 2812-1), humidity chamber (ISO 6270), salt chamber (ISO 7253) to durability range: HIGH. Matches the SSPC paint 20 (type II)
Can be applied in several layer for ongoing recoat able maintenance, up to one year open time for recoating without any surface preparation. The primer is a metallic paint containing zinc, Lead-free, without chromates or coal tar. The anti corrosive Epoxy primer is a metallic gray strong paint with low surface tension with excellent adhesion especially to ferrous metals.
Properties:
- Anticorrosive high build primer paint, enriched with zinc, provides a cold galvanization (cathode protection) against rust.
- A primer paint with mechanical strength and excellent adhesion to ferrous metals.
- Form a proper preparation for painting with aliphatic polyurethane top coat.
- Can be recoat in many layers with open recoating time until one year.
- Resistant to harsh and corrosive conditions including extremely wet and salty environment.
- Excellent adhesion to the infrastructure, bridging between an old proper paint to a new top paint.
- Easy to apply, dries rapidly.
- Thixotropic and suitable for spraying thick coat in every layer.
- Ready for recoating and/or top coating in the same day after 8 hours.
- High coverage ability.
- Durable in fuels and oils.
- Suitable for maintenance painting in electric stations.
Epoxyden Primer Zinc Enrich Cold Galvanization
Epoxyden primer Zinc enrich anticorrosive recoatable
Applications:
- As a primer coat for polyurethane or others top coat paints in maintenance works for fixing mechanical hits or for total painting without possibility/time for appropriate surface preparation.
- For painting iron and galvanized steel constructions
- For painting pipes and tankers for production and/or storage.
- and For painting iron apparatus, devices, facilities, buildings and/or their legs for corrosion protection especially in salt sea or other corrosive environment. .
- For painting machines and machines parts.
- As primer before top coat for any iron surfaces that are not worming over 100O
Technical data:
- Theoretical coverage in 25 micron dry layer – 1 liter for 25 sqm.
- Practical coverage – 1 liter for 4.3-6.4 sqm..
- Hiding power – a layer of 58 microns > 0.95
- Flexibility – 1 mm (Sheen)
- Density –part A =1.35-1.55 gm\cm3 part B =0.85-0.95 gm\cm3(ASTM D1475)
- Viscosity part A + part B immediately after mixing – 40 seconds # 4
- Hardness – >10 Dg (Erickson)
- Flash point – 27OC
- Solids by volume – mixed A+B= 65% by Vol., 81% by weight, (ASTM-D-2369)
- Erosion – CS-17 wheel, (ASTM D4060), 1000 cycles with 1 kg. load – weight loss 200 mg.
- Recommended layer thickness – 100-150 microns dry, 150-225 microns wet.
- Recommended number of layers – at least 1 (surface passive – can apply many coats)
- Touch-drying time Up to 15 minutes, no sticky time – 30 minutes.
- Hard drying time – up to 8 hours.
- Pot life (working time from mixing a with b) – 4-6 hours. (After 4 hours blend B + A viscosity less than 70 seconds on cup 4 # after 8 hours will not show jell)
- Mixing ratio A: B – 1 : 1 by volume.
Epoxyden primer Zinc enrich anticorrosive recoatable
- Waiting time after mixture and before painting: 10 minutes. And stir again with a mechanical mixer before start painting.
- Heat resistance- for 1 hr. in 121oc without changes of shade or quality of the film.
- Hot oil durability – 121oc for 24 hours without any changes in the quality of the film and the shade.
- Oil hydraulic resistance point- 65oc for 24 hours without any changes in the quality of film and it shade.
- Solvents durability – 50 cycles rubbing with cloth soaked in MEK – no peeling of paint.
- Distilled water resistance – 4 days in 49oc – no defects of film and adhesion.
- Non salts water resistance – 6 months deeping – stick 3M standard tape to surface under pressure of 2 kg and after 1 hr. pull it off – no paint split off the surface.
- Conductivity test, Microsiemens microS/cm instrument AP-2, compare result in start deeping and after 6 months with no changes.
- Adhesion test after 7 drying days – stick 3M standard tape to surface under pressure of 2 kg and after 1 hr. pull it off – no paint split off the surface.
- Pull off adhesion test after 7 drying days – 1050 Psi (ASTM D 4541)
- Salt spray (with scratch) resistance – 3000 hr. (development corrosion up tp 5 mm ASTM B117-97 table 1 step 5)
Epoxyden primer Zinc enrich anticorrosive recoatable
- Salt spray test according ISO 7253 – 1440 hours with scratch 5 cm. and at list 2 cm from edge of panel (3 panels test 7×15 cm.) M= C-W=1 and will not be more than ½.
- 2 2
C – size of scratch with rust W- size of scratch 50 mm
Test on 250 micron film – there will not be any paint splits, bubbles, or any other defects. Corrosion level will not go over 1 mm.
- Humidity cabinet 720 hr. 30 cycles for high durability (ISO 6270) there will not be any paint splits, bubbles, or any other defects.
- Chemical resistance – (ISO 2812-1) 168 hours with no defects on the film. Check in NaOH 10%, H2SO4 10%, Turpentine mineral with 18% aromatics. Foe the tests: Lm-1 water, Lm-2 sodium chloride 5%.
Epoxyden Primer Zinc Enrich Cold Galvanization
Epoxyden primer Zinc enrich anticorrosive recoatable
Contains:
- Epoxy resin and polyamide hardener.
- Fillers, anticorrosive pigments.
- Polyamide hardeners.
- Solvents and additives
Colors:
- Grayish.
Gloss:
- Matt < 5% (ASTM D 523) 60O lens test
Touch dry time:
- 15 minutes. (Due to the quick drying time avoid from over spray, avoid spraying “dust”)
Drying between layers:
- 6-8 hours. Final drying: 8 hours.
Application methods:
- Brush, roller, spray.
- Spray gun – it is recommended inter pressure > 4 atm.
- Airless – dilution 0-5% nozzle 0.021 “
Thinning:
- Thinner D-4/100. (MIL-T-81771 Type II)
- 10-25% by volume -according to need. if orange peel appearance you can increase the dosage to 35%
- Spraying with spry gun – 10-25%
- Airless – 0-5% pressure 3-5 atm. nozzle 0.018”-0.021” pressing piston ratio: 30:1 minimum.
Epoxyden Primer Zinc Enrich Cold Galvanization
Epoxyden primer Zinc enrich anticorrosive recoatable
Surface preparation:
- A thorough cleaning needed from dirt, dust and loose paints.
- On old paint – sand well and clean with air pressure, clean with dry clean cloth soaked with thinner.
- Iron Metals – recommended but not must – sand blast cleaning till white metal appears SA-2.5 level. Metal brushes clean -For rusty surfaces ST-3, for light rusty surfaces – ST-2.5, for galvanize steel – sanding until totally matte surface appears.
- Very big surfaces –remove the paint with paint removers and wash with water for neutralizing. Sand/spray soft sands or plastic powder for light roughness. Rinse with water and dry completely.
- For aluminum –burn with ANTAROX 4 and PASSIVATOR 1722 yellow/green, or spray layer of Epoxyden Stronzium Chromate MIL–C-23377 for best primer and this product Epoxyden zinc enrich as mid. Thick layer.
Primer:
- This product itself.
Epoxyden primer Zinc enrich anticorrosive recoatable
Top color:
- You can paint the top layer 8-12 hours after painting the primer if it had the heat and dryness condition.
- During the cold winter, you can paint only after 24 hours.
- The top layer can be “Denbergloss” aliphatic exterior polyurethane paint with UV resistance.
Instructions for use:
- Open carefully parts A and B and stir separately.
- Pour from two parts in the right ratio the required amount and mix well with mechanical mixer (operated by air pressure is recommended for safety reasons) for a uniform mixture.
- Wait for 10 minutes while adding the thinner as needed and mix again. Spray a thick layer of 150-225 microns thickness 100-150 mic. dry film if no licks appear. If necessary if the layer does not completely uniform or part of surface not painted, wait about 4-12 hours for complete drying and spray another layer. Insert into clean and controlled temp. drying room for 12 hours before painting the top layer.
- Wash the equipment well immediately after finishing painting.
Pot Life after mixing the mixture a + b of 5 liters:
- 15oc – 10 hr.
- 20oc – 8 hr.
- 25oc – 7 hr.
- 30oc – 6 hr.
- 35oc – 4 hr.
Epoxyden Primer Zinc Enrich Cold Galvanization
Epoxyden primer Zinc enrich anticorrosive recoatable
Ventilation:
- Quantity air needed for 1 liter of blend paint :
- Achieving 10% of the LEL = 65M3
- To obtain the TLV = 990 M3
Packaging:
- 2.5+ 2.5 = 5 liters.
Storage:
- In cool and shaded room in room temp. with proper ventilation.
- Keep lids tightly closed.
Shelf life:
- 24 months in original package.
Tools cleaning:
- D- 4/100 thinner immediately after painting.
Quality control:
- In factory laboratories according to specifications.
- COA and COC certificate.
- ISO 9001-2015
Safety precautions:
- Inedible, keep away from the reach of children.
- Flammable – keep distant from heated areas, fires, flames, and sparks, Prohibit smoking in working area.
- While applying, good air ventilation is important. In case there is not enough air, use ventilation according to the ventilation table.
- Wear protective glasses, gloves and suits.
- Avoid direct contact of the paint and/or thinner with the eyes and skin. In case of contact, immediately wash thoroughly with water.
- In case of an injury immediately get doctors assistance.
- Read the safety instructions on the labels.
- See M.S.D.S
Epoxyden Primer Zinc Enrich Cold Galvanization
Epoxyden primer Zinc enrich anticorrosive recoatable
- Visit our sites: www.denber-paints.co.il
- www.denber-colors.co.il
- Varnish for wood. How to choose the right varnish for wood
- Thermal isolation Thermoseal 200 energy saving in green construction
- Crystal epoxy resin for tables
- Fire resistance of houses, hardwood and parquet floors, decks
- Sealing the floor of the balcony, terrace from rain
- Thin floor nano-coverings for industrial refrigerators and freezers
- Epoxy floors – Benefits of epoxy floors
- Swelling paints for steel protection against fire – Fire retardant paint
- As part of the restoration of buildings – concrete restoration at the Yad Kennedy site
- Paint for aircraft Denbergloss Jets
- Complicated sealing based on innovative technologies
- Reconstruction project of a unique house (Israeli house of architect Gaudi); Renovation of condominiums
- The work on the floor covering and restoration of the sports hall has been completed
- Denber has developed an innovative solution for thermal insulation works
- Mold, how to remove mold correctly and how to fight mold
- “Sick” buildings – Antibacterial paints destroys viruses / bacteria – Bacterinoll/ Tutgum Bacterinol
- Denber – floor coating using epoxy and polyurethane – find out what is suitable for you epoxy floor or polyurethane floor
- Epoxy floor coating and epoxy paints