Epoxyden PA and DU/Zn galvanized primer

Epoxyden PA and DU/Zn galvanized primer

EPOXY PRIMER PAINT FOR GALVANIZED STEEL.

Epoxyden PA and DU/Zn galvanized primer. www.denber-paints.co.il

Epoxyden PA and DU/Zn galvanized primer. www.denber-paints.co.il

Epoxyden PA & DU/Zn is two a component Epoxy primer paint suitable especially as primer for galvanized steel (hot and cold galvanization). It is based on special resins and pigments providing excellent adhesion to the galvanized metals. Creates a strong basis, which is the first condition, for stable top painting on galvanized steel,

Properties

  • Excellent adhesion to galvanized steel.
  • A strong and durable primer for top paints.
  • It has excellent mechanical strength.
  • Resistant to scratches.
  • Resistant to diluted alkali or acids as well as to extreme humidity.
  • Durable for dry heat up to 200OC for short exposure time.
  • Suitable as primer paint for various top paints such as polyurethane, epoxy, chlorinated rubber, syntactic etc.
  • Easy to apply, dries quickly.
  • High coverage as a very thin layer needed.
  • Durable in fuels, oils, jet fuels etc.

Epoxyden PA and DU/Zn galvanized primer

EPOXY PRIMER PAINT FOR GALVANIZED STEEL.

Applications:

  • Primer paint for galvanized steel.
  • Primer paint for constructions made of galvanized steel, and elements from galvanized steel in industrial uses.
  • Primer for galvanized steel for aviation uses.

Technical data:

  • Theoretical coverage – 1 liter to 12-15 sqm.
  • Coverage according layer thickness – 10-15 sqm.
  • Recommended layer thickness – 10-35 microns dry, recommended 20 microns per layer. (minimum values)
  • Recommended number of layers –2
  • Mixing ratio, A: B – 1: 1 by volume.
  • Adhesion to Galvanized steel and Aluminum – 180 kg/cm2
  • Viscosity part A + part B immediately after mixing – 1-2 Pa.sec (Haake)
  • Flexibility – 1 mm (sheen)
  • Density –part A =1.1-1.2gm\cm3 (ASTM D1475) (DIN 53452)
  • Hardness – >3 Dg (Erichsen)
  • Flash point – 38OC
  • Stretch resistance – 400 kg/cm2.
  • Impact resistance -1.8 Dg/mm2
  • Pressing resistance – 600 kg/cm2
  • Bending resistance – 30 N/mm2
  • Pot life (working time from mixing a with b) – 8 hours in 20OC
  • Erosion-120 microns film – 2800 cycles (BYK Gardner) ASTM (loss of 66 mg ASTM 4060 for 120 mics. dry film with wheel cs-17 loaded 1 kg.)
  • Elasticity in drag – 10% N/ mm2 (DIN 53455)
  • Resistance to drag – 3 N/mm2 (DIN 53455)
  • Touch-drying time 4-6 hours.
  • Hard drying time – up to 24 hours.
  • Waiting time after mixture and before painting: 10 minutes. And stir again with a mechanical mixer before start painting.

Epoxyden PA and DU/Zn galvanized primer

EPOXY PRIMER PAINT FOR GALVANIZED STEEL.

Temperature Time
15°C 30 min.
20°C 15 min.
25°C 10 min.
  • Heat resistance – for 1 hr. in 121OC without changes of shade or quality of the film.
  • Hot oil durability – 121OC for 24 hours without any changes in the quality of the film and the shade.
  • Oil hydraulic resistance point- 65OC for 24 hours without any changes in the quality of film and it shade.
  • Solvents durability – 50 cycles rubbing with cloth soaked in MEK – no peeling of paint.
  • Distilled water resistance – 4 days in 49OC – no defects of film and adhesion.
  • Adhesion test – stick 3M standard tape to surface under pressure of 2 kg and after 1 hr. pull it off – no paint split off the surface.
  • Paint removing – 90% and more within 60 minutes in paint remover.
  • Salt spray resistance – 2000 hr.

Contains:

  • Epoxy resin and polyamide hardener. (tiny molecular size)
  • Adhesion promoters.
  • Wetting agents.
  • Zinc chromate.
  • Flexibility improvers.
  • Solvents and additives

Colors:

  • Grey,
  • Red brown
  • Brown.

Epoxyden PA and DU/Zn galvanized primer

EPOXY PRIMER PAINT FOR GALVANIZED STEEL.

Gloss:

  • Matt < 5% (ASTM D 523) 60O lens test

Touch dry time:

  • : 4-6 hours.
  • Final: 24 hr.

Drying time between layers:

  • 16 hours. Dry too hard for painting on it: 48 hr. (un that case a sanding needed and a new layer of Epoxyden wash primer). Final hardness: 7 days.
Temp. 5°C 10°C 15°C 20°C 30°C 40°C
First curing 16h. 8h. 5h. 4h. 3h. 2h.
Final curing None 15 days 10 days 7 days 3 days 2 days

Application methods:

  • Brush, roller, spray.

Thinning:

  • Thinner D-4/100. (MIL-T-81771 Type II)
  • Brushing/roller – 5%
  • Spraying – 10-20% by volume –pressure 3-4 atm. nozzle 1.6
  • Airless – 0% ratio piston 30:1 inlet pressure 4-5 atm. nozzle 0.015-0.018” outlet pressure 120-150 atm.

Surface preparation:

  • A thorough cleaning needed from dirt, dust and loose paints.
  • Galvanized steel – sand lightly to remove light oxidation and/or gloss and clean with air pressure, clean with dry clean cloth soaked with thinner/acetone.
  • Very old galvanization with rust – sand blast for total removing of rust.

Epoxyden PA and DU/Zn galvanized primer

EPOXY PRIMER PAINT FOR GALVANIZED STEEL.

Primer:

  • This product itself.

Top color:

  • You can paint the top layer 8-12 hours after painting the primer if it had the heat and dryness condition.
  • During the cold winter, you can paint only after 24 hours.
  • The top layer can be “Denbergloss” aliphatic exterior polyurethane paint with UV resistance.

Instructions for use:

  • Open carefully parts A and B and stir separately.
  • Pour from two parts in the right ratio the required amount and mix well with mechanical mixer (operated by air pressure is recommended for safety reasons) for a uniform mixture.
  • Wait for 15 minutes while adding the thinner as needed and mix again. Spray a thin layer of at least 20 microns thickness dry film. If necessary if the layer does not completely uniform or part of surface not painted, wait about 4-12 hours for complete drying and spray another layer. Insert into clean and controlled temp. drying room for 12 hours before painting the top layer.
  • Wash the equipment well immediately after finishing painting.

Pot Life after mixing the mixture a + b of 5 liters:

  • 15oc – 10 hr.
  • 20oc – 8 hr.
  • 25oc – 7 hr.
  • 30oc – 5 hr.
  • 35oc – 4 hr.

Ventilation:

  • Quantity air needed for 1 liter of blend paint:
  • Achieving 10% of the LEL = 65M3
  • To obtain the TLV = 990 M3
  • Quantity air needed for 1 liter of thinner 4/100:
  • Achieving 10% of the LEL = 182M3
  • To obtain the TLV = 2125 M3

Epoxyden PA and DU/Zn galvanized primer

EPOXY PRIMER PAINT FOR GALVANIZED STEEL.

Packaging:

  • 2.5+2.5 = 5 liters. 5+5=10 liters.

Storage:

  • In cool and shaded room in room temp. with proper ventilation.
  • Keep lids tightly closed.

Shelf life:

  • 12 months in original package.

Tools cleaning:

  • D- 4/100 thinner immediately after painting.

Quality control:

  • In factory laboratories according to specifications.
  • COA and COC certificate.
  • ISO 9001-2015

Safety precautions:

  • Inedible, keep away from the reach of children.
  • Flammable – keep distant from heated areas, fires, flames, and sparks, prohibit smoking in working area.
  • While applying, good air ventilation is important. In case there is not enough air, use ventilation according to the ventilation table.
  • Wear protective glasses, gloves and suits.
  • Avoid direct contact of the paint and/or thinner with the eyes and skin. In case of contact, immediately wash thoroughly with water.
  • In case of an injury immediately get doctors assistance.
  • Read the safety instructions on the labels.
  • See M.S.D.S

Epoxyden PA and DU/Zn galvanized primer

EPOXY PRIMER PAINT FOR GALVANIZED STEEL.